NusEce TransitionMetal plastics Polyimide semifluorinated_alkane FrictionForce PinpointPFM HBN Adhesive piezoelectric force microscopy Growth Optic PetruPoni_Institute frequency_modulation GlassTemperature fifber TemperatureControllerStage KAIST Mfm BiFeO3 Vacuum LateralForceMicroscopy BismuthVanadate PECurve EFM thermal_conductivity Neodymium HighResolution Grain TemperatureControlledAFM Pyroelectric Logo Oxidation Ito ScanningKelvinProbeMicroscopy
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Self-assembly of Semi-fluorinated Alkanes
Domains formed by the self-assembly of semi-fluorinated alkanes deposited as a monolayer on the surface of the water. The monolayer was compressed before being transferred onto a silicon substrate. Each domain includes about 4000 molecules. The domains were easily detached from the substrate with tapping mode because the molecules were very loosely attached to the substrate. Only Non-contact mode could achieve this result.
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: PPP-FMR (k=2.8N/m, f=75kHz)
- Scan Size: 1μm×1μm, 0.5μm×0.5μm, 0.2μm×0.2μm
- Scan Rate: 2Hz
- Pixel Size: 500 × 500
- Scan Mode: Non-contact
- Cantilever: PPP-FMR (k=2.8N/m, f=75kHz)
- Scan Size: 1μm×1μm, 0.5μm×0.5μm, 0.2μm×0.2μm
- Scan Rate: 2Hz
- Pixel Size: 500 × 500