Piezoresponse STM P3HT Magnetostrictive ferromagnetic Optoelectronic Yttria_stabilized_Zirconia CarbonNanotube Sulfur Blend Spain FrictionalForceMicroscopy PMNPT LateralForce WPlug Hafnium_dioxide Domain BiVO4 Morphology SiliconOxide CalciumHydroxide Mechinical MolybdenumDisulfide CuFoil strontiu_titanate Fet Electronics HfO2 Optic self-assembled_monolayer Permalloy LiquidImaging thermal_conductivity conductive Blood
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Hard Disk Media
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: SSS-NCHR (k=42N/m, f=300kHz)
- Scan Size: 1μm×1μm, 0.3μm×0.3μm
- Scan Rate: 0.5Hz, 1Hz
- Pixel Size: 512×512, 256×256
- Scan Mode: Non-contact
- Cantilever: SSS-NCHR (k=42N/m, f=300kHz)
- Scan Size: 1μm×1μm, 0.3μm×0.3μm
- Scan Rate: 0.5Hz, 1Hz
- Pixel Size: 512×512, 256×256