Glass NeodymiumMagnets PolymerBlend SKPM MESA structure Writing 2d_materials polymeric_arrays SurfaceOxidation Modulus PiezoelectricForceMicroscopy CHRYSALIS_INC Mechanical molecular_self_assembly AnodizedAluminumOxide Yttria_stabilized_Zirconia FailureAnalysis Lift VortexCore Fujian tip_bias_mode Conductive AFM Reading ContactModeDots CompactDisk FuelCell 2dMaterials fluoroalkane CopperFoil exfoliate MagneticPhase SelfAssembly BismuthVanadate neodymium_magnets FrictionalForceMicroscopy
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Crystal
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: NCHR
- Scan Size: 2μm×2μm
- Scan Rate: 0.7Hz
- Pixel: 256 × 256
- Scan Mode: Non-contact
- Cantilever: NCHR
- Scan Size: 2μm×2μm
- Scan Rate: 0.7Hz
- Pixel: 256 × 256