ElectroChemical Step AmplitudeModulation Metal Ferroelectric PhaseImaging MagneticArray Tape TungstenDeposition FloppyDisk NUS_NNI_Nanocore Blend Liquid NUS_Physics Gallium Force-distance PolyStylene Leakage FAFailureAnlaysis Polydimethylsiloxane kelvin probe force microscopy CancerCell Memory SelfAssembly fluorocarbon Alkane GaN Graphene Bmp Worcester_Polytechnic_Institute Display #Materials Nanopattern Organic ContactMode
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
MoS2
Scanning Conditions
- System: NX10
- Scan Mode: KPFM
- Cantilever: NSC36C Cr-Au(k=0.6N/m, f=65kHz)
- Scan Size: 12μm×12μm
- Scan Rate: 0.15Hz
- Pixel:256×256
- Scan Mode: KPFM
- Cantilever: NSC36C Cr-Au(k=0.6N/m, f=65kHz)
- Scan Size: 12μm×12μm
- Scan Rate: 0.15Hz
- Pixel:256×256