PFM mechanical_property TyphimuriumBiofilm BaTiO3 DeflectionOptics PyroelectricDetector bias_mode Laser AmplitudeModulation LiIonBattery Floppy Ram SiliconOxide DNA Fet MembraneFilter StainlessSteel PhaseChange Self-assembledMonolayer Aluminum CHRYSALIS_INC PS_LDPE tip_bias_mode CeramicCapacitor ThermalDetectors CBD Hexacontane India OpticalWaveguides ThermalConductivity Neodymium plastics thermal_conductivity Lift Nanofiber
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Block copolymer thin film
Scanning Conditions
- System: NX10
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm, 1μm×1μm
- Scan Rate: 0.5Hz, 1Hz
- Pixel: 512×512, 512×512
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm, 1μm×1μm
- Scan Rate: 0.5Hz, 1Hz
- Pixel: 512×512, 512×512