Cobalt-dopedIronOxide ElectroChemical Polypropylene Neodymium StrontiumTitanate Copolymer Annealing Ananth CP-AFM Polyethylene Polymer Film BCZT MagneticPhase Oxidation Barium_titanate TungstenThinFilmDeposition SurfaceOxidation solar_cell NUS CVD Polystyrene IcelandSpar frequency_modulation Subhajjit Electical&Electronics self-assembly silicon_carbide Mechanical SurfaceChange cross section P3HT AdhesionEnergy LiftMode hard_disk_media
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
MoS₂ film
Scanning Conditions
- System : FX40
- Scan Mode: Tapping
- Scan Rate : 1Hz
- Scan Size : 40μm×40μm
- Pixel Size : 512×256
- Cantilever : OMCL-AC160TS (k=26N/m, f=300kHz)