Modulus Vinylpyridine Calcite silicon_oxide Strontium HighAspect Hysteresys HfO2 InorganicCompound TemperatureControllerStage TemperatureControlledAFM NUS_Physics Roughness PhthalocyaninePraseodymium KAIST PinPointMode ForceVolume Glass Layer Domain Sic Pores DIWafer HighResolution Conduct Reading Switching thermal_property NCM\ FuelCell Grain PinpointNanomechanicalMode PtfeFilter OpticalWaveguide Yeditepe_University
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
HOPG
Scanning Conditions
- System: NX20
- Scan Mode: FM-KPFM
- Cantilever: qpBioAC AuCB1 (k=0.3N/m, f=90kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 256
- Scan Mode: FM-KPFM
- Cantilever: qpBioAC AuCB1 (k=0.3N/m, f=90kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 256