Alloy MultiLayerCeramicCapacitor Vanadate KAIST BreastCancerCell Morphology I-VSpectroscopy Tin sulfide BTO BaTiO3 UnivCollegeLondon piezoelectric force microscopy temp PatternedSapphireSubstrat TemperatureControlledAFM OpticalWaveguide Fendb ScanningKelvinProbeMicroscopy Au111 Multiferroic_materials Neodymium HafniumDioxide Pinpoint Ucl OrganicSemiconductor DentalProsthesis PolyimideFilm StrontiuTitanate Yeditepe_University ito_film BiasMode Chemical_Vapor_Deposition TungstenDeposition MoS2 Piezo
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Red Blood Cell
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: ACTA (k=40N/m, f=300kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.5Hz
- Pixel: 256×256