Gallium_Arsenide Jason MagneticForce Hexatriacontane Blood PhthalocyaninePraseodymium HexagonalBN Nanotechnology PVAC Bacteria ForceVolume Foil H-BN HardDiskMedia HighResolution Bmp ScanningKelvinProbeMicroscopy Boron PANI Magnetic Force Microscopy PiezoelectricForceMicroscopy Kevlar Polypropylene norganic Global_Comm CeNSE_IISc VerticalPFM Praseodymium Ptfe Treatment Hair WS2 FrequencyModulation UnivMaryland LFM
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
PP/LDPE polymer blend
Scanning Conditions
- System: NX20
- Scan Mode: Pinpoint mechanical
- Cantilever: FMR (k=2N/m, f=75kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.35Hz
- Pixel: 256×256
- Modulus calculation model: Hertzian