Composition Bmp Adhesion Forevision Christmas norganic single_layer HanyangUniv MagneticPhase Wafer MfmPhase EFMAmplitude Lanthanum_aluminate Patterns Adhesive ScanningKelvinProbeMicroscopy ChemicalCompound KelvinProbeForceMicroscopy HexacontaneFilm Piezoresponse BTO Magnetic Hydroxyapatite Silver MLCC UnivOfMaryland PolymerPatterns cannabis ShenYang FailureAnlaysis Treatment SICM VinylAlcohol DIWafer SicMosfet
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
BN thin film on Si
Scanning Conditions
- System: NX10
- Scan Mode:SThM
- Cantilever: Nanothermal probe
- Scan Size: 25μm×25μm, 5μm×5μm
- Scan Rate:0.3Hz, 0.5Hz
- Pixel: 256×256, 256×256
- Scan Mode:SThM
- Cantilever: Nanothermal probe
- Scan Size: 25μm×25μm, 5μm×5μm
- Scan Rate:0.3Hz, 0.5Hz
- Pixel: 256×256, 256×256