EFM Sperm HardDiskMedia Permalloy Barium_titanate atomic_layer Iron BiFeO3 Multiferroic_materials Pvdf MultiLayerCeramicCapacitor Film TemperatureControllerStage Bismuth heterojunctions OpticalModulator Electrode SKPM Microchannel Cobalt cannabidiol IISCBangalore Heating #Materials rubber Inorganic BiVO4 Steps small_scan WS2 ElectroDeposition Lanthanum_aluminate Ferroelectric Nickel sputter
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Polymer blend with nanofiber
Scanning Conditions
- System: NX10
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.5Hz
- Pixel: 512×512
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.5Hz
- Pixel: 512×512