Chemical Vapor Deposition Hole OrganicCompound Pipette Switching AEAPDES Composition molecules contact ForceVolumeImage LightEmission Multiferroic_materials Blend INSP SurfaceChange TPU fifber Holes tip_bias_mode Tungsten_disulfide ScanningIon-ConductanceMicroscopy Carbon Semiconductor bias_mode Polyaniline optoelectronics Calcite GranadaUniv Dental Cobalt conductive Genetic Chungnam_National_University NiFe PvdfFilm
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Block copolymer ΙΙ
Scanning Conditions
- System: NX10
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 2μm, 0.3μm, 0.1μm
- Scan Rate: 1Hz, 1Hz, 2Hz
- Pixel: 512×512, 256×256, 256×256
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 2μm, 0.3μm, 0.1μm
- Scan Rate: 1Hz, 1Hz, 2Hz
- Pixel: 512×512, 256×256, 256×256