LateralForceMicroscopy Piezoelectric GalliumPhosphide STM Ferrite Butterfly Conductivity FrictionForce SICM PtfeFilter block_copolymer CalciumHydroxyapatite HexacontaneFilm INSP NeodymiumMagnets Chungnam_National_University phase_change SrTiO3 BiVO4 AM_KPFM DNAProtein LightEmission Zhi Biology CuFoil MfmAmplitude Yttria_stabilized_Zirconia Mechinical mfm_amplitude Wildtype FFM BTO Ni-FeAlloy Composition AlkaneFilm
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
PDMS liquid crystal
Scanning Conditions
- System: NX10
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 15μm×15μm
- Scan Rate: 0.5Hz
- Pixel: 512×512
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 15μm×15μm
- Scan Rate: 0.5Hz
- Pixel: 512×512