CuFoil AM_KPFM MultiferroicMaterials SiliconOxide FrictionalForce OrganicCompound 3-hexylthiophene MetalCompound plastic Temasek_Lab Ferrite PhaseTransition Bacterium HighAspect HafniumDioxide DataStorage HOPG LateralForce thermal_property Polytetrafluoroethylene Aluminium_Oxide Melt FailureAnalysis EFM Sadowski SmalScan Praseodymium Wildtype Vinylpyridine Laser BloodCell Growing 2d_materials Array Implant
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Adhesive system
Scanning Conditions
- System: NX10
- Scan Mode: PinPoint
- Cantilever: ACST (k=7N/m, f=150kHz)
- Scan Size: 30μm×30μm, 20μm×20μm
- Scan Rate: 0.23Hz
- Pixel: 256×256
- Scan Mode: PinPoint
- Cantilever: ACST (k=7N/m, f=150kHz)
- Scan Size: 30μm×30μm, 20μm×20μm
- Scan Rate: 0.23Hz
- Pixel: 256×256