AnodizedAluminumOxide GlassTemp AdhesionEnergy Floppy Mapping PFM Modulus BiasMode CuSubstrate Molybdenum_disulfide OrganicSemiconductor Chromium PANI LateralForceMicroscopy Conductive AFM cannabidiol VinylAlcohol MonoLayer PolymerBlend temperature_control Bmp Magnetostrictive Ceramics Growing exfoliate FailureAnlaysis margarine SetpointMode hetero_structure Croatia ContactMode NCM\ Epoxy 3-hexylthiophene MagneticForceMicroscopy
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Gold(111) coated mica substrate
Scanning Conditions
- System: XE7
- Scan Mode: Contact
- Cantilever: PPP-ContScR (k=0.2N/m, f=25kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 1Hz
- Pixel: 256×256
- EC electrode: Ag/AgCl2(Reference electrode), Pt(Counter electrode), CuSO4(0.1mM) + H2SO4(0.01mM)(Electrolyte)
- EC bias voltage: -0.3V