Wildtype Zhi NusEce align suspended_graphene LiquidImaging GaP SRAM SoftSample Neodymium #EC LDPE CompactDisk Inorganic_Compound LFM Growth PvdfBead nanobar Piezoresponse AnodizedAluminumOxide Ecoli FAFailureAnlaysis Fe_film Cancer PFM Tin disulfide TriGlycineSulphate HexagonalBN PrCurve Layer lift_mode chemical_compound domain_switching temperature_control Thermal
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Cast Iron surface change after Corrosion
Scanning Conditions
- System: NX10
- Scan Mode: Contact
- Cantilever: NSC36C (k=0.6N/m, f=65kHz)
- Scan Size: 50μm×50μm
- Scan Rate: 1.5Hz
- Pixel: 512×1024
- EC bias voltage: -0.266V