Melt ImideMonomer Bacterium StyreneBeads light_emitting doped CrystalGrowing Piezo SingleLayer MultiLayerCeramicCapacitor LifeScience SmalScan PinpointNanomechanicalMode EvatecAG ScratchMode plastics SKPM Nanostructure Biology electrospinning WPlug FrictionalForce TPU SolarCell mfm_amplitude thermal_property gallium_nitride Electical&Electronics ReflexLens Wildtype P3HT Growth heterojunctions LithiumNiobate BariumTitanate
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
HOPG Moire
Scanning Conditions
- System: NX10
- Scan Mode: STM
- Cantilever: Pt wire
- Scan Size: 2.5μm×2.5μm, 0.5μm×0.5μm, 0.2μm×0.2μm
- Scan Rate: 0.3Hz, 1Hz, 2Hz
- Pixel: 512×256, 512×256, 256×128
- Scan Mode: STM
- Cantilever: Pt wire
- Scan Size: 2.5μm×2.5μm, 0.5μm×0.5μm, 0.2μm×0.2μm
- Scan Rate: 0.3Hz, 1Hz, 2Hz
- Pixel: 512×256, 512×256, 256×128