ElectroChemical Chungnam_National_University PiezoelectricForceMicroscopy AdhesionForce ScanningSpreadingResistanceMicroscopy Step SingleCrystal Magnetic FailureAnlaysis StrontiumTitanate Pinpoint SetpointMode Electrical&Electronics fluoroaalkane Praseodymium Cobalt Potential Pores Blend TCS Blood MBE MoirePattern Hexylthiophene Oxidation PMNPT ReflexLens SSRM ThermalDetectors Plug Korea HanyangUniv Hair Graphite Permalloy
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
MoS2
Scanning Conditions
- System: NX10
- Scan Mode: AM-KPFM
- Cantilever: ElectriMulti75 (k=3 N/m, f=75kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.5Hz
- Pixel: 256×256