DLaTGS IcelandSpar norganic NUS_NNI_Nanocore FrictionalForceMicroscopy NUS GranadaUniv Nickel DOE Corrosion BTO Permalloy GalliumPhosphide suspended_graphene ScanningTunnelingMicroscopy TungstenDeposition Hair Jason Reduction FrequencyModulation AIN Piranha Domain CBD ElectroDeposition Change ForceVolumeImage LiftHeight InsulatorFilm ULCA AdhesionEnergy Annealing atomic_layer Austenite Magnetostrictive
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Polymer patterns on Si (1/2)
Scanning Conditions
- System: NX10
- Scan Mode: KPFM
- Cantilever: NSC36Cr-Au (k=1N/m, f=90kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.2Hz
- Pixel: 512×256