flakes MeltingPoint Boundary I-VSpectroscopy Aggregated_molecules HOPG lithography ReflexLens Au111 Cell Butterfly Flake silicon_carbide AmplitudeModulation PtfeMembrane Korea FM-KPFM PinPointMode KelvinProbeForceMicroscopy Domain Led Battery Electrical&Electronics ContactMode Regensburg EvatecAG block_copolymer Crystal AIN Oxide Litho Composite 2-vinylpyridine Polyvinylidene Leakage
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
BFO (BiFeO3)
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 10μm×10μm, 5μm×5μm
- Scan Rate: 0.8Hz, 0.8Hz
- Pixel: 512×512, 512×512