Bio Mobile IISCBangalore temperature_control OpticalElement India ShenYang Hysteresys PS_LDPE GaP Silver CntFilm doped SoftSample Sadowski Heating PinpointPFM hydrocarbon Fe_film dielectric_trench Ananth Hexatriacontane Piezoresponse IcelandSpar LiIonBattery Butterfly UnivCollegeLondon AtomicSteps Polyvinylidene optoelectronics MLCC LifeScience LithiumNiobate LiquidImaging self-assembly
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
ExFoliated graphene on SiO₂/Si wafer
Scanning Conditions
- System : FX40
- Scan Mode: Non-Contact, Lithography
- Scan Rate : 1 Hz
- Scan Size : 10μm×10μm
- Pixel Size : 256×256
- Cantilever : PPP-EFM (k=2.8N/m, f=75kHz)
- Litho. Condition : Force 200nN, Writing speed 0.2 μm/s , AC bias 10 V @ 40 kHz, Humidity ~90% RH