Titanate Phosphide Calcium Ananth India C36H74 organic_polymer Liquid ConductingPolymer FM_KPFM Crystal NCM Annealed Fluoride silicon_oxide vertical_PFM Aluminum LiftHeight #Materials Force-distance light_emitting rubber high_resolution Pipette temperature controller AFM Plug SKPM self_assembly Chemical_Vapor_Deposition Nickel AtomicSteps Dental Granada DIWafer Fiber
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Defects of Reflex lens
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.5Hz
- Pixel: 512×512