Melt FailureAnalysis Polyvinylidene_fluoride Nanotechnology DomainSwitching Tungsten_disulfide Materials PVAP3HT flakes Flake UTEM CompactDisk Vacuum Boron CarbonNanotube Kevlar atomic_layer nanomechanical Piezo Imprint Tin sulfide Bio Sadowski Magnetostrictive Worcester_Polytechnic_Institute HafniumDioxide NTU NCM\ Mechanical LiftMode IMT_Bucharest Pore Calcium Edwin MagneticArray
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
NCA of Li-ion battery (2/2)
Scanning Conditions
- System : NX-Hivac
- Sample bias: 1 V
- Scan Mode: SSRM
- Scan Rate : 0.25Hz
- Scan Size : 15μm×15μm
- Pixel Size : 256×256
- Cantilever : AD-40-AS (k=40N/m, f=200kHz)