Sapphire Bmp Aggregated_molecules SPMLabs plastics Wafer LiquidImaging blended polymers Lateral_Force_Microscopy 2d_materials Cross-section Granada block_copolymer Sphere PMNPT Holes Epoxy Fe_film LiquidCell Indium_tin_oxide FuelCell Polystyrene ImideMonomer sputter Blood thermal_conductivity Tungsten StyreneBeads ito_film FloppyDisk FrictionalForce WPlug Display PetruPoni_Institute MolybdenumDisulfide
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Fe-Nd-B
Scanning Conditions
- System: NX20
- Scan Mode: Non-contact, TCS
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.5Hz
- Pixel: 512×256
- TCS: Temperature control stage type2