Regensburg Yttria_stabilized_Zirconia I-VSpectroscopy Polyethylene FM_SKPM AnodizedAluminumOxide Typhimurium SRAM Litho SICM TiO2 Transparent multi_layer Galfenol Vacuum Titanate Moire C36H74 SrO Polypropylene SmallScan Ecoli PolycrystallineFerroelectricBCZT Heating LiNbO3 HydroGel Cell Magnetic Force Microscopy ThermalDetectors Cancer Foil INSP Nickel Pattern Sio2
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Polymer-Ceramic composite
Scanning Conditions
- System: NX10
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 3μm×3μm
- Scan Rate: 0.4Hz
- Pixel: 512×256