flakes Permalloy BismuthVanadate ReflexLens Change LiquidCrystal ScanningSpreadingResistanceMicroscopy Inorganic Techcomp Pore CeNSE_IISc RedBloodCell layers AEAPDES Step Collagen #Materials HafniumDioxide CuFoil HydroGel Solar Forevision Liquid Oxidation plastic Memory self_healing Morphology polyvinyl acetate DataStorage Tapping HBN Litho Conductivity Wang
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
CMP test key
Scanning Conditions
- System : NX20
- Scan Mode: Non-contact
- Scan Rate : 1Hz for 25μm2 / 0.6HZ for 15μm2
- Scan Size : 25μm2, 15μm2
- Pixel Size : 512×256 for 25μm2 / 1025×128 for 15μm2
- Cantilever : PPP-NCHR (k=42N/m, f=330kHz)