Chloroform PolyvinylideneFluoride Ucl Magnets PMNPT lift_mode BaTiO3 SoftSample InLiquid strontiu_titanate TungstenDeposition Christmas ElectrostaticForceMicroscopy MechanicalProperties StyreneBeads Pinpoint PFM Strontium Ferrite PolyvinylAcetate silicon_oxide HafniumDioxide atomic_steps PECurve KPFM MonoLayer TipBiasMode dichalcogenide margarine Stiffness SurfaceChange SolarCell MBE optoelectronics Fet Electrode
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Escherichia coi (E. coli)
Scanning Conditions
- System : NX10
- Scan Mode: Non-contact
- Scan Rate : 0.5 Hz
- Scan Size : 20μm×20μm
- Pixel Size : 256×256
- Cantilever : PPP-NCHR (k=42N/m, f=330kHz)