MagneticForce Permalloy Tin sulfide Silver dichalcogenide Temperature CompactDisk InsulatorFilm polymeric_arrays AM_KPFM MagneticPhase SICM Polyimide Pipette lithography LateralForce Ceramics Tin disulfide KelvinProbeForceMicroscopy align domain_switching IndiumTinOxide Hair Heating Graphite HBN cannabis Mosfet Sadowski Electrical&Electronics hard_disk VerticalPFM NusEce PtfeFilter polyvinyl acetate
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Semiconductor device, Failure analysis
Scanning Conditions
- System: NX10
- Scan Mode: Conductive AFM
- Cantilever: CDT-Contr (k=0.5N/m, f=20kHz)
- Scan Size: 11μm×11μm
- Scan Rate: 1Hz
- Pixel: 512×512
- Sample bias: -0.5V