TransitionMetal Imprint molecular_beam SurfaceChange fifber Pzt Organic Chrome Polydimethylsiloxane Growth Film BreastCancerCell GranadaUniv high_resolution SRAM atomic_layer fluoroaalkane Solar Mosfet Change PvdfBead epitaxy VerticalPFM Aggregated_molecules Sapphire cooling Carbon Magnetic thermal_property F14H20 Jason cross section Scanning_Thermal_Microscopy CrossSection CuParticle
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Nanostructures on polymer
Scanning Conditions
- System : NX10
- Scan Mode: Non-contact
- Scan Rate : 0.5 Hz
- Scan Size : 5μm×5μm
- Pixel Size : 256×256
- Cantilever : PPP-NCHR (k=42N/m, f=330kHz)