MechanicalProperties Reading ContactMode ThinFilm LateralPFM sputter PhaseImaging TiO2 MolybdenumDisulfide Regensburg Corrosion DiffractiveOpticalElements Optical Wildtype UnivMaryland Cancer Materials Multiferroic_materials domain_switching InLiquid Bismuth ImideMonomer EFMAmplitude Polytetrafluoroethylene ForceDistanceSpectroscopy Metal-organicComplex Polyurethane Tin disulfide PolycrystallineFerroelectricBCZT contact YszSubstrate Lateral BismuthVanadate EFM CalciumHydroxyapatite
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Defect of LinbO₃
Scanning Conditions
- System : FX40
- Scan Mode: Non-contact
- Scan Rate : 0.3 Hz
- Scan Size : 10μm×10μm
- Pixel Size : 1024×512
- Cantilever : SCOUT 350 (k=42N/m, f=350kHz)