TPU Plastic Thin Film

TPU Plastic Thin Film

Thermoplastic polyurethane (TPU) is polyurethane plastics with many properties, including elasticity, transparency, and resistance to oil, grease and abrasion.

Scanning Conditions

- System: NX20
- Scan Mode: Pinpoint
- Cantilever: PPP-CONTSCR (k=0.2N/m, f=25kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.28Hz
- Pixel Size: 256 × 256