LDPE MagneticForce PECurve Mobile Piezoresponse Fluoride PetruPoni BoronNitride molecular_beam Phthalocyanine FloppyDisk Melt MembraneFilter Sic Change OpticalModulator BreastCancerCell Tungsten temp_control Glass non_contact Anneal Force-distance Zagreb TemperatureControllerAFM Electrical&Electronics single_layer Potential CopperFoil Polyurethane Oxide Copper HighResolution Holes PinpointPFM
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
PS/LDPE
Spincast layer of PS/LDPE blend on Si.
Scanning Conditions
- System: NX20
- Scan Mode: Tapping
- Cantilever: AD40AS (k=40N/m, f=180kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 256
- Scan Mode: Tapping
- Cantilever: AD40AS (k=40N/m, f=180kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 256