LDPE MoirePattern Polypropylene Oxide Change PFM LightEmiting ForceMapping Lift STM Litho flakes CeramicCapacitor MultiLayerCeramicCapacitor Fluoride GaP FAPbI3 Cross-section block_copolymer Dr.JurekSadowski LFM MultiferroicMaterials Indium_tin_oxide Writing pinpoint mode SetpointMode StainlessSteel MolecularSelfAssembly SmalScan EvatecAG SICM Defects HfO2 Wang FM_SKPM
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
C36H74
Layer of C36H74 alkane on HOPG.
Scanning Conditions
- System: NX20
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 256
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 256