CuFoil Ucl Cobalt Domain CrossSection Modulus polyvinyl acetate Spincast Floppy OxideLayer kelvin probe force microscopy Sperm Wildtype Friction molecules Display Insulator DIWafer Annealing Filter LDPE Permalloy TransitionMetal IIT-chennai FM_KPFM Glass Dr.JurekSadowski ContactModeDot GlassTemp ContactModeDots Tungsten VortexCore Mosfet medical SelfAssembly
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
F14H20
Semifluorinated alkanes on Si.
Scanning Conditions
- System: NX20
- Scan Mode: Tapping
- Cantilever: AD40AS (k=40N/m, f=180kHz)
- Scan Size: 5μm×5μm, 1μm×1μm
- Scan Rate: 05Hz, 1Hz
- Pixel Size: 1024 × 512, 512 x 256
- Scan Mode: Tapping
- Cantilever: AD40AS (k=40N/m, f=180kHz)
- Scan Size: 5μm×5μm, 1μm×1μm
- Scan Rate: 05Hz, 1Hz
- Pixel Size: 1024 × 512, 512 x 256