STO Co/Cr/Pt Vortex MagneticPhase Epoxy LateralPFM temp_control Heat SiliconOxide C_AFM Deposition Sio2 Phase Reading TungstenThinFilmDeposition tip_bias_mode OpticalWaveguide Polarization DOE FailureAnlaysis exfoliate Growing SingleCrystal PinpointNanomechanicalMode IMT_Bucharest Korea block_copolymer Optoelectronic Grain Polymer HafniumDioxide strontiu_titanate Friction AmplitudeModulation Liquid
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
MoS2
Scanning Conditions
- System: NX10
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 25μm×25μm
- Scan Rate: 0.8Hz
- Pixel Size: 512 × 256
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 25μm×25μm
- Scan Rate: 0.8Hz