Vac Scratch Force-distance Materials nanomechanical Solution Conductive AFM Mechanical&nanotechnology Conduct Transparent Fiber Patterns Ito CeramicCapacitor frequency_modulation LDPE OpticalElement Wildtype exfoliate MechanicalProperties BlockCopolymer Ram #Materials PhaseTransition MoirePattern PpLdpe Electrode margarine Polydimethylsiloxane fluorocarbon Polyimide ring shape Blood DeoxyribonucleicAcid ElectrostaticForceMicroscopy
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
PVDF Fibrous Membrane
PVDF fibrous membrane made by electrospinning.
Scanning Conditions
- System: NX10
- Scan Mode: Pinpoint PFM
- Cantilever: PPP-EFM (k=2.8N/m, f=75kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.05Hz
- Pixel Size: 256 × 256
- Scan Mode: Pinpoint PFM
- Cantilever: PPP-EFM (k=2.8N/m, f=75kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.05Hz
- Pixel Size: 256 × 256