Anneal HBN EvatecAG Aluminium_Oxide DLaTGS H-BN Tape TCS Electical&Electronics TemperatureControlledAFM NUSNNI Ptfe IIT-chennai Graphite PFM HiVacuum TungstenThinFilmDeposition Pattern Yeditepe Calcium Wonseok Varistor Jason KelvinProbeForceMicroscopy Tungsten_disulfide NUS INSP MolecularSelfAssembly Cobalt-dopedIronOxide BariumTitanate HafniumDioxide Bio Reading Neodymium fluoroaalkane
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Fe-Nd-B Alloy
Scanning Conditions
- System: NX10
- Scan Mode: MFM
- Cantilever: PPP-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 15μm×15μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 256
- Lift height: 100nm
- Scan Mode: MFM
- Cantilever: PPP-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 15μm×15μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 256
- Lift height: 100nm