AtomicLayer small_scan SolarCell Protein Friction Polarization Multiferroic_materials PVA PolymerPatterns molecule SiliconeOxide CuFoil Galfenol hard_disk Bacterium neodymium_magnets VerticalPFM Defects Tapping ito_film Writing PyroelectricDetector Polyaniline Sapphire Sulfur PinpointNanomechanicalMode Electical&Electronics 2dMaterials norganic atomic_layer ItoGlass LaAlO3 Terrace AAO Regensburg
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
ER 316L Stainless Steel
The ferrite MFM phase has a striped appearance due to its ferromagnetic behavior, while the paramagnetic austenite phase shows a uniform appearance.
Scanning Conditions
- System: NX20
- Scan Mode: AM-KPFM, MFM
- Cantilever: PPP-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 20μm×20μm
- Scan Rate: 0.3Hz
- Pixel Size: 512 × 512
- Lift height: 30nm
- Scan Mode: AM-KPFM, MFM
- Cantilever: PPP-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 20μm×20μm
- Scan Rate: 0.3Hz
- Pixel Size: 512 × 512
- Lift height: 30nm