Blend hard_disk optoelectronics Fluoride Battery Dental Formamidinium_lead_iodide Phthalocyanine Optoelectronic alkanes Hexylthiophene fifber NUSNNI membrane Filter SKPM Imprint oxide_layer Solution Gallium ItoGlass Chloroform mfm_amplitude Wang electrospinning Collagen VortexCore Mobile TungstenDeposition Al2O3 Vacuum TemperatureControlledAFM Permalloy FAPbI3 PS_PVAC
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
CVD Grown WS2
Scanning Conditions
- System: NX10
- Scan Mode: AM-KPFM
- Cantilever: NSC36Cr-Au A (k=1N/m, f=90kHz)
- Scan Size: 17μm×17μm
- Scan Rate: 0.3Hz
- Pixel Size: 512 × 256
- Scan Mode: AM-KPFM
- Cantilever: NSC36Cr-Au A (k=1N/m, f=90kHz)
- Scan Size: 17μm×17μm
- Scan Rate: 0.3Hz
- Pixel Size: 512 × 256