OrganicSemiconductor Protein SKPM Hafnium_dioxide LithiumNiobate IVSpectroscopy Polyaniline Microchannel Materials BloodCell Flake SolarCell MechanicalProperties HACrystal Graphite TPU PDMS CntFilm Change Epoxy PS_PVAC graphene_hybrid SrTiO3 Thermoplastic_polyurethane Fet PANI EvatecAG Magnetostrictive PolyStylene StyreneBeads LiIonBattery MonoLayer ContactModeDots PolyvinylAcetate OpticalWaveguides
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
MoS2 Layers on SiO2
A few layers of MoS2 on SiO2
Scanning Conditions
- System: NX10
- Scan Mode: AM-KPFM
- Cantilever: NSC36Cr-Au B (k=2N/m, f=130kHz)
- Scan Size: 30μm×30μm
- Scan Rate: 0.3Hz
- Pixel Size: 512 × 256
- Scan Mode: AM-KPFM
- Cantilever: NSC36Cr-Au B (k=2N/m, f=130kHz)
- Scan Size: 30μm×30μm
- Scan Rate: 0.3Hz
- Pixel Size: 512 × 256