Sidewall Modulus Croatia Polyaniline DOE MolecularSelfAssembly Ni81Fe19 SPMLabs Permalloy Beads C60H122 Dr.JurekSadowski semifluorinated alkane CaMnO3 AdhesionEnergy Conduct Calcite CP-AFM Au111 IISCBangalore PinPointMode Sperm C_AFM StainlessSteel Sic Annealed BFO Layer UnivOfMaryland MagneticArray Materials dielectric_trench Holes LFM Electronics
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Trench Etch Profile on MESA
Top dielectric trench etch profile on MESA on Si wafer.
Scanning Conditions
- System: NX20
- Scan Mode: Non-contact
- Cantilever: AR5T-NCHR (k=42N/m, f=300kHz)
- Scan Size: 6μm×6μm
- Scan Rate: 0.12Hz
- Pixel Size: 1024 × 256
- Scan Mode: Non-contact
- Cantilever: AR5T-NCHR (k=42N/m, f=300kHz)
- Scan Size: 6μm×6μm
- Scan Rate: 0.12Hz
- Pixel Size: 1024 × 256