CuParticle Litho TiO2 SelfAssembly Worcester_Polytechnic_Institute Defect pulsed_laser_deposition Dr.JurekSadowski Indent piezoelectric force microscopy Magnetic Force Microscopy Bio Fujian C60H122 Vortex CrystalGrowing light_emitting polymeric_arrays DLaTGS BFO Organic Water Multiferroic_materials Switching MBE Boundary flakes Au111 strontiu_titanate Magnets thermoplastic_elastomers BlockCopolymer dielectric trench Flake Moire
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
AlN/GaN/AlN Hetero Structure
AlN/GaN/AlN hetero structure grown on SiC substrate by Molecular Beam Epitaxy (MBE) system.
Scanning Conditions
- System: NX20
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 512
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 512