temp_control Collagen Boundary CarbonNanotube TappingMode Neodymium DomainSwitching layers Vortex Platinum Transparent mfm_amplitude MetalCompound FailureAnlaysis align FrictionalForceMicroscopy FloppyDisk BismuthFerrite Roughness Wildtype cannabidiol Sadowski FM-KPFM Graphene strontiu_titanate EPFL Ananth Alkane MfmAmplitude LMF Tape pinpoint mode Holes Metal-organicComplex thermoplastic_elastomers
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
ITO Film Sputter Deposited onto Silicon
ITO-film, which was sputter deposited onto silicon. The grain size of those samples was influenced by changing the process settings in the Cluterline RAD sputter deposition system, one of the deposition tool platforms manufactured by Evatec.
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: PPP-EFM (k=2.8N/m, f=75kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.1Hz
- Pixel Size: 256 × 256
- Scan Mode: Non-contact
- Cantilever: PPP-EFM (k=2.8N/m, f=75kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.1Hz
- Pixel Size: 256 × 256