Current SelfAssembly Sidewall Granada Biofilm UTEM light_emission HACrystal Carbon GranadaUniv CrystalGrowing UnivMaryland ReflexLens GaAs Sphere margarine self_assembly Titanate HighAcpectRatio AM_KPFM mono_layer Resistance temp_control OrganicCompound membrane SurfaceOxidation AM-KPFM FM_KPFM MultiferroicMaterials Filter AlkaneFilm Change Steps Crystal InLiquid
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Perovskite
Scanning Conditions
- System: NX10
- Scan Mode: KPFM
- Cantilever: NSC36A Cr-Au (k=1N/m, f=90kHz)
- Scan Size: 4μm×4μm
- Scan Rate: 0.3Hz
- Pixel: 512×256