HBN UnivOfMaryland HOPG LDPE AtomicSteps Implant cannabidiol Optoelectonics HighAcpectRatio PolyvinylideneFluoride FM_KPFM Graphite PolyvinylAcetate hetero_structure Blood Roughness Defect Step Leakage Spincast Photovoltaics Aluminum Chemical Vapor Deposition CalciumHydroxyapatite Adhesive PetruPoni_Institute electrospinning FM_SKPM PolyStylene Tungsten_disulfide Bacteria MechanicalProperty DiffractiveOpticalElements ElectroChemical norganic
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Polymer (2/2)
Scanning Conditions
- System: NX10
- Scan Mode: Tapping
- Cantilever: NCHR
- Scan Size:1μm×1μm
- Scan Rate: 1Hz
- Pixel: 256 × 256
- Scan Mode: Tapping
- Cantilever: NCHR
- Scan Size:1μm×1μm
- Scan Rate: 1Hz
- Pixel: 256 × 256