Chloroform China Perovskite Hafnium_dioxide PvdfBead CalciumHydroxide Conductance Optoelectonics PinPointMode LowDensityPolyethylene HfO2 Cancer Molybdenum_disulfide OpticalWaveguides University_of_Regensburg lift_mode DNAProtein Polyimide HardDiskMedia MfmPhase MolecularSelfAssembly NiFe mechanical property HighAcpectRatio Bio MechanicalProperty NtuEee Polyvinylidene_fluoride Singapore Polytetrafluoroethylene SetpointMode OrganicCompound dielectric_trench Electronics Christmas
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
BTO
Scanning Conditions
- System: XE7
- Scan Mode: DC-EFM(Vertical)
- Cantilever: ElectriMulti75G (k=3N/m, f=75kHz)
- Scan Size: 20μm×20μm
- Scan Rate: 0.2Hz
- Pixel: 256×256
- Sample Bias: 0V
- Tip Bias: 1V ac
- Scan Mode: DC-EFM(Vertical)
- Cantilever: ElectriMulti75G (k=3N/m, f=75kHz)
- Scan Size: 20μm×20μm
- Scan Rate: 0.2Hz
- Pixel: 256×256
- Sample Bias: 0V
- Tip Bias: 1V ac