Au111 KPFM DNA Gallium_Arsenide block_copolymer light_emitting CalciumHydroxyapatite TyphimuriumBiofilm Piezo Battery IVSpectroscopy LightEmission Scanning_Thermal_Microscopy IMT_Bucharest BFO Biology LiftHeight Ecoli Metal-organicComplex Change Beads Sperm single_layer HardDiskMedia contact HighAcpectRatio fluorocarbon TungstenThinFilmDeposition kelvin probe force microscopy 3-hexylthiophene LithiumNiobate Heat Stiffness Hysteresys Piezoresponse
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
MoS2
Scanning Conditions
- System: NX10
- Scan Mode: KPFM
- Cantilever: NSC36C Cr-Au(k=0.6N/m, f=65kHz)
- Scan Size: 12μm×12μm
- Scan Rate: 0.15Hz
- Pixel:256×256
- Scan Mode: KPFM
- Cantilever: NSC36C Cr-Au(k=0.6N/m, f=65kHz)
- Scan Size: 12μm×12μm
- Scan Rate: 0.15Hz
- Pixel:256×256