FastScan vertical_PFM Celebration Biology Zagreb OpticalModulator SingleCrystal Anneal Electronics GaN Metal ContactModeDot Nanostructure norganic Cancer LogAmplifier Molybdenum_disulfide atomic_layer Imprint Sulfur Mobile Cobalt amplitude_modulation OrganicCompound ScratchMode AdhesionEnergy Phthalocyanine Bmp Calcite BCZT HanyangUniv Polyvinylidene_fluoride MagneticArray exfoliate 3-hexylthiophene
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Carbon Nanotube on Si
Scanning Conditions
- System: XE7
- Scan Mode: SThM, KPFM, PinPoint CP-AFM
- Cantilever: Nanothermal probe, NCST-Au (k=7.4N/m, f=160kHz), CDT-CONTR (k=0.5N/m, f=20kHz)
- Scan Size: 0.6μm×0.6μm
- Scan Rate: 0.5Hz, 0.5Hz, 0.15Hz
- Pixel: 256×128
- Scan Mode: SThM, KPFM, PinPoint CP-AFM
- Cantilever: Nanothermal probe, NCST-Au (k=7.4N/m, f=160kHz), CDT-CONTR (k=0.5N/m, f=20kHz)
- Scan Size: 0.6μm×0.6μm
- Scan Rate: 0.5Hz, 0.5Hz, 0.15Hz
- Pixel: 256×128