ScanningSpreadingResistanceMicroscopy Polymer Roughness mfm_amplitude SelfAssembly Foil lift_mode neodymium_magnets I-VSpectroscopy LateralPFM PolyvinylAcetate Pinpoint PFM Phthalocyanine Friction PolyStylene MoS2 Magnetostrictive Imprint single_layer Sic piezoelectric force microscopy MetalCompound MultiLayerCeramicCapacitor Boundary KAIST thermoplastic_elastomers Gallium LiquidCell heterojunctions SiliconCrystal self_healing India FrictionForce high_resolution Composite
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Christmas ball lithography on Si substrate
Scanning Conditions
- System: NX10
- Scan Mode: Contact, lithography
- Cantilever: : ContscPt (k=0.2N/m, f=25kHz)
- Scan Size: 30μm×30μm
- Scan Rate: 0.5Hz
- Pixel: 512×512