Glass Polyimide Solar Subhajjit Defect GaP CastIron Collagen Copolymer STO bias_mode PolymerPatterns contact BismuthVanadate PolyimideFilm block_copolymer Austenite FrequencyModulation plastics OrganicSemiconductor HydroGel chemical_compound thermoplastic_elastomers ElectroChemical Ni81Fe19 Biology C_AFM Electrode ContactModeDot NUS DiffractiveOpticalElements DataStorage Dopped CuFoil Boundary
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Atomic steps on GaP(Gallium Phosphide) layer on Si
Scanning Conditions
- System: NX20
- Scan Mode: Non-contact
- Cantilever: PPP-NCHR (k=42N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 1Hz
- Pixel: 512×512